 5公斤氟钠钠。 In the leaching step, each cubic meter of ammonia - ammonium sulfate solution was added 0. 3~0. 5kg sodium fluorosilicate. The purpose is to make the ammonia leaching reaction easier and more thorough. Adding an appropriate amount of sodium fluorosilicate can break the package of zinc-containing particles by a kind of ultrafine particles such as calcium hydroxide formed during the dissolution and conversion process of calcium sulfate in the ammonia solution. , the ultra-fine particles are layered and peeled off to achieve leaching.

...

Inductively coupled plasma-optical emission spectrometry (ICP-OES) is another popular method for determining barium in TiO2. This technique uses an inductively coupled plasma to ionize the sample and then measures the intensity of light emitted by the resulting ions. ICP-OES offers high sensitivity and wide dynamic range, allowing for the detection of trace amounts of barium. It also requires specialized equipment, but its automation capabilities can reduce costs and improve efficiency.

...
...