In addition to quality, CL77891 also offers a wide range of titanium dioxide products to cater to different applications
...
2025-08-14 21:17
1324
The calcined product obtained by the ordinary zinc-barium white preparation method is beaten into a slurry, which is then surface-treated with sodium silicate, aluminum sulfate or sodium aluminate and surfactant, and then filtered, washed, dried and pulverized. Can.
Edelweiss, 14.5 per cent zinc sulphide, 84 per cent barium sulphate, 1.5 per cent carbonate of lime.