Thirdly, titanium dioxide is a semiconductor material with a wide bandgap energy of 3
...
2025-08-14 10:18
2677
The reaction liquid is filtered through plate and frame pressure to obtain lithopone in the form of a filter cake with a moisture content of no more than 45%. It is then roasted in a drying furnace to change the crystal form of lithopone, and is then pickled with sulfuric acid at a temperature of 80°C. Finally, it is washed with water, reinforced with colorants, filtered, dried and ground into powder.