use of titanium dioxide manufacturers

Natural barite and anthracite containing more than 95% barium sulfate are mixed and fed at a ratio of 3:1 (mass). After being crushed to a diameter of less than 2cm, it enters the reduction furnace. The furnace temperature is controlled to be 1000-1200°C in the front section and 500-500 in the back section. 600°C, the reduction furnace rotates at a speed of 80 seconds per revolution, and the reaction conversion rate is 80% to 90%.

...

Titanium dioxide production begins with the extraction of raw materials, typically ilmenite or rutile, from mines. In a white titanium dioxide factory, these minerals undergo a rigorous refining process that includes steps like sulfuric acid digestion, chloride process, or sulfate process, depending on the factory's technology and resources. The resulting titanium dioxide pigment is then purified, dried, and ground to achieve the desired particle size and quality.

...