2025-08-14 15:45
388
This route affords a product that is 29.4 wt % ZnS and 70.6 wt % BaSO4. Variations exist, for example, more ZnS-rich materials are produced when zinc chloride is added to the mixture of zinc sulfate and barium sulfide.
The calcined product obtained by the ordinary zinc-barium white preparation method is beaten into a slurry, which is then surface-treated with sodium silicate, aluminum sulfate or sodium aluminate and surfactant, and then filtered, washed, dried and pulverized. Can.