titanium dioxide in coatings manufacturers

Washed with ethanol nZnS-BaS0 4 crystalline cake, washing the filter cake drying cabinet at 105 ° C after drying lh pulverized by atomic absorption detection zinc, barium yield, in order to reach 98.4% based on zinc, barium meter 99%, ZnS mass fraction accounted for 36.6%. The total mass fraction of zinc sulfide and barium sulfate reached 99.22%, and the mass fraction of ZnS accounted for 36.6%. The particle size of barium sulfide is larger than that of zinc sulfide, which is 77 nm and 38 calendars respectively. The indicators of tinting strength and oil absorption exceed the GB/T1707-1995 B311 type.

...

Lithopone’s historical significance is further accentuated by the advancements and modifications that followed its inception. The 1874 patent by J.B. Orr, for instance, ushered in a new white pigment—Orr’s Zinc White. This innovation was attained by co-precipitating zinc sulfate and barium sulfide, followed by a calcination process. Further refinements marked the subsequent decades, the most notable being the enhancement of lightfastness achieved in the 1920s by introducing small amounts of cobalt salts before calcination.

...