1. 296 to 1.357 g/cm3 is obtained. The reaction solution is subjected to pressure filtration through a plate frame to obtain a cake-like lithopone powder having a water content of not more than 45%. The mixture is calcined in a dry roaster to change the crystal form of the lithopone, and then acid-washed with sulfuric acid at a temperature of 80 °C. Finally, it is washed with water, reinforced with coloring agent, pressure filtration, drying and milling.

...

Developing new Lithopone formulations, one that enhances the properties of the existing Lithopone is anticipated to boost the demand for Lithopone white pigment during the forecast period. Reinforced Lithopone is one such development, wherein a copolymer is added to the polymerization reaction to yield Lithopone with an increased weather resistance and an anti-ultraviolet property. Moreover, development of nano-scale Lithopone is also anticipated to attract market interest during the forecast period.

...