2339
The reaction liquid is filtered through plate and frame pressure to obtain lithopone in the form of a filter cake with a moisture content of no more than 45%. It is then roasted in a drying furnace to change the crystal form of lithopone, and is then pickled with sulfuric acid at a temperature of 80°C. Finally, it is washed with water, reinforced with colorants, filtered, dried and ground into powder.
The application of lithopone in building materials industry can not only be used as water-soluble coatings for interior and exterior walls of buildings, but also as fillers for wallpaper, floor paint, dining table and other plastic all ceramic veneers.