lithopone b301 suppliers

 At present, Lide powder is mainly produced in China. Most of the domestic Lide powder production is still using traditional methods. The main raw materials are zinc oxide, sulfuric acid and barium sulfide (barite and coal are produced by high temperature reduction). Zinc 45% ~ 70%. The traditional method for producing the Liede powder process is to use zinc bakelite containing more than 45% zinc as a raw material to be leached with sulfuric acid to obtain a crude zinc sulfate solution, and then to remove iron by potassium permanganate, and then replace the heavy metal with zinc powder and filter to obtain zinc sulfate. The refined liquid is further subjected to metathesis reaction, pressure filtration, calcination, rinsing, drying, and pulverization with strontium sulfide to obtain a series of different types of lindose powder containing zinc sulfide of 30% or more. The whole process is carried out in an acidic (ra<7) environment, which consumes a large amount of sulfuric acid. The sulfuric acid has strong corrosiveness and requires high production equipment. The final discharged slag is acidic slag, which brings new pollution to the environment. High requirements, high production costs, and poor quality of the products obtained.

...

The primary function of TiO2 in pigment production is its exceptional ability to provide brightness and opacity. When added to paints or coatings, it enhances their hiding power by reflecting light back to the observer's eye. This property not only improves the aesthetic appeal of the product but also reduces the amount of colorant needed, resulting in cost savings for manufacturers. Moreover, TiO2's high refractive index ensures that even small quantities can significantly impact the final appearance of the product.

...

Here, NaOH or NH3 · H2O is used as a precipitant or pH regulator to react with FeSO4 to form ferrous hydroxide precipitation; Air is used as oxidant; The iron sheet reacts with sulfuric acid produced during the oxidative hydrolysis of FeSO4 to provide ferrous ions required in the reaction system and maintain the pH value of the solution. The alkali consumption of acid method is less and the particles are easy to wash. The relative rates of seed preparation and crystal growth determine the particle size, particle size distribution and particle morphology of iron yellow particles.

...