tio2 technology

2. Barite calcination method A solution of barium sulfide is prepared. The sulfuric acid and zinc oxide are reacted, purified by adding potassium permanganate and zinc powder, and compressed to obtain a zinc sulfate solution. Then, the prepared barium sulfide solution is mixed and subjected to a metathesis reaction to obtain a mixture of zinc sulfide and barium sulfate, and then the precipitate is subjected to pressure filtration, calcination, wet grinding, drying, and pulverization to obtain a zinc white product.

...

Although barium sulfate is almost completely inert, zinc sulfide degrades upon exposure to UV light, leading to darkening of the pigment. The severity of this UV reaction is dependent on a combination of two factors; how much zinc sulfide makes up the pigments formulation, and its total accumulated UV exposure. Depending on these factors the pigment itself can vary in shade over time, ranging from pure white all the way to grey or even black. To suppress this effect, a dopant may be used, such as a small amount of cobalt salts, which would be added to the formulation. This process creates cobalt-doped zinc sulfide. The cobalt salts help to stabilize zinc sulfide so it will not have as severe a reaction to UV exposure.

...