Natural barite and anthracite containing more than 95% barium sulfate are mixed and fed at a ratio of 3:1 (mass). After being crushed to a diameter of less than 2cm, it enters the reduction furnace. The furnace temperature is controlled to be 1000-1200°C in the front section and 500-500 in the back section. 600°C, the reduction furnace rotates at a speed of 80 seconds per revolution, and the reaction conversion rate is 80% to 90%.
Looking ahead, the future of China's titanium oxide industry looks promising, as the demand for the pigment continues to grow across various sectors. With its abundant resources, advanced technology, and commitment to sustainability, China is well-positioned to remain a key player in the global titanium oxide market for years to come.