1. 296 to 1.357 g/cm3 is obtained. The reaction solution is subjected to pressure filtration through a plate frame to obtain a cake-like lithopone powder having a water content of not more than 45%. The mixture is calcined in a dry roaster to change the crystal form of the lithopone, and then acid-washed with sulfuric acid at a temperature of 80 °C. Finally, it is washed with water, reinforced with coloring agent, pressure filtration, drying and milling.

...

3) Metathesis reaction: Dissolve the sulfide in distilled water to obtain a clear decomposition liquid, and add nonionic surfactant to stir evenly, then slowly add it to the zinc sulfate ammonia complex solution to form a metathesis reaction, and obtain Lide powder opacity. The liquid is separated by filtration, and the separated ammonia liquid is returned to the leaching after ammonia adjustment, and the separated nZnS-BaS0 4 crystal filter cake is put into the next step;

...
...